Dear Sadique,
                      We cannot do painting on the weleed joints before hydrotest, only after hydrotest the painting on the welded joints should be performed & the surface preparation  is ST2 hand tool cleaning.

Regards,
Sajan
Painting QC
NSH Corp

On Mon, Feb 9, 2009 at 10:31 AM, sadique sheikh <mails_sadique@yahoo.com> wrote:
HI ALL OF U
My question is can we do painting of welded joints of pipe before hydro test?ALSo plz give me the reference of that.
Regards
Sadique Sheikh





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...