Sunday, February 8, 2009

[MW:1510] Re: NDT after hydrotest for ASME Sec VIII Div 2 vessels

nothing as per ASME sec VII Div.2 no requirement

On 2/8/09, Raghuram Bathula <raghurambathula@gmail.com> wrote:

Is there any NDT requirement after hydrotest in Section VIII div2 for
any material?

Thanks in adv.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...