[MW:1491] Re: Cladding Pipe Manufacturer

Check WSI (Welding Services Inc) in Atlanta GA USA

Original Message:
-----------------
From: Paresh Katvi pkatvi@gmail.com
Date: Sun, 1 Feb 2009 12:51:45 +0400
To: materials-welding@googlegroups.com
Subject: [MW:1489] Re: Cladding Pipe Manufacturer


You cn check with EEW Germany.

Regards

On Thu, Jan 8, 2009 at 2:00 PM, <rahul.pisat@akersolutions.com> wrote:

> Sirs,
>
> Can anybody guide me for Cladded Pipe manufacturers ?
> I am looking for clad pipe manufacturer with weld overlay manufacturing
> process or a Mechanical bonding cladding.
>
> The required material is 30" Pipe with X70 grade CS and SS316L grade
> cladding.
>
> Waiting for information.
>
> Kind reg
> *Rahul Pisat*
> *Engineer - Material Engineer*
>
> This e-mail and any attachment are confidential and may be privileged or
> otherwise protected from disclosure. It is solely intended for the
person(s)
> named above. If you are not the intended recipient, any reading, use,
> disclosure, copying or distribution of all or parts of this e-mail or
> associated attachments is strictly prohibited. If you are not an intended
> recipient, please notify the sender immediately by replying to this
message
> or by telephone and delete this e-mail and any attachments permanently
from
> your system.
> >
>


--------------------------------------------------------------------
mail2web.com – Enhanced email for the mobile individual based on Microsoft®
Exchange - http://link.mail2web.com/Personal/EnhancedEmail

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

Anonymous said...

Hello,

Maybe Fronius can help you.
They different solutions for cladding equipment.

best regards

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...