Dear Santosh Karnire,

With thanks for your explanations but as you see on subject of my mail, I mean this connection as branch connection ( 3/4"x 4" ).

I'm waiting for your valuable comments.


Best Regards,

On Sun, Jan 16, 2011 at 3:31 PM, Santosh Karnire <skarnire@permapipe.ae> wrote:

Dear Zarei,

 

Srinivasulu is correct , it is not advisable.

 

Reason being – There will be a drastic reduction(i.e from 4" to ¾" ), leading to sudden change in Pressure and velocity of the fluid being transmitted, leading to safety issue.

 

Gap as wide as 40mm on each side is too large to be filled up by welding and I doubt if it is commercially viable. Concentric Reducer is will more cheaper and will be easier to weld to the main pipe I.e 4inch.    

 

Best Regards,

Santosh Karnire
Purchase Engineer



P.O. Box 4988, Fujairah, United Arab Emirates. www.permapipe.ae
Tel   : +971 9 2282540 Ext: 139   |   
Fax    : +971 9 2282541
Cell  : +971 55 6471359              |   Email : skarnire@permapipe.ae

**** Setting the international standard for Pre-insulated Pipe for the District Cooling and Oil & Gas Industries.


This message, including any attachments, may contain confidential information & may also be legally privileged. The information contained in this e-mail message is intended only for the use of the rightful & intended addressee & must not be disclosed to any third party without express permission. If you are not the intended recipient, you are hereby notified that any distribution, copying, review, retransmission, dissemination or other use of this electronic transmission or the information contained in it is strictly prohibited. If this email is received in error, no confidentiality or privilege is waived or lost. Please notify the sender or email contactus@permapipe.ae & delete the email you have received from your system & destroy any hard copy.

From: Srinivasulu Kalasapati [mailto:nirgunaya@gmail.com]
Sent: Sunday, January 16, 2011 11:26 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:0] BRANCH 3/4" FROM 4" LINE LP STEAM

 

Usually it's not advisable to do that so.

On Sat, Jan 15, 2011 at 5:02 PM, ENAYAT ZAREI <zarei.enayat@gmail.com> wrote:

Dear All,

Is it possible to weld pipe 3/4" to pipe 4" in LP steam service  in the form of Pipe to Pipe (we have no any sockolet or Halfcoupling, ...)?

Does it need REINFOCEMENT?

your reply is highly appreciable.

 

Regards

Zarei

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Ohm Guru Namasivaya

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...