Wednesday, January 5, 2011

Re: [MW:9107] WPS and PQR for P 1 material and P 5

Dear Krishna,

Please explain your query in detail,
if you are qualifying PQR then you can always choose different filler metals for different passes or If you have WPS which mention different filler metal for Cap, Also the title is vague "WPS and PQR for P 1 material and P 5", Please clarify.

Regards
Manpreet Singh


On Wed, 05 Jan 2011 16:59:32 +0530 Saamy wrote
>Dear All !
> Could you help me any one... We have IS 2062 material
>for rail welding... the manufacturer recommend for E 7018 for root,
>hot and filling and E9018 for capping on IS 2062... My Question is how
>to allow E 9018 on IS 2062? Both electrodes have different A No...
>That is essential variable... So please give advice...
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...