[MW:9200] RE: 9171] API 530 Solution annealing after coiling of SA213 TP304H

Mr. Karthik,
 
What's the design code, API-530 or API-560?
 
I browsed through both the documents(2002/2004 editions),API- 530 is more of a calculation/design guideline while 560 is looks to be a design and fabrication specification.
 
Thanks.
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Specialist & Consultant
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthik
Sent: Monday, January 10, 2011 9:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:9171] API 530 Sollution annealing after coiling of SA213 TP304H

Dear All,
Please give your views on below quirey.
Material: SA213 TP304H- Tube-Dia-101.6x8.55mm
Code: API530.
The above material has sollution annealed at 1040 degree celsius from material manufacturer.We are going to make coiling of these tubes(Coil Dia-3.5Mx8M(height) ).
Quirey:
01. Does sollution annealing to be done again after coiling of these tubes? because our customer asked us to do Sollution annealing after coiling.(they referred to ASME Sec.II-Part-A)Also our customer not aware of API530 requirements.Also I dont have API530 book.
 
02.Please give, is there is any requirement as per API530?

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...