[MW:5103] RE: 955] RE: 954] CC2235 UT in lieu of RT and the name plate marking

Further to following discussion I would like opinion of members for the name plate marking in case a vessel is only ultrasonically tested.

UG 116(e) states "When radiographic or ultrasonic examination has been performed on a vessel in accordance with UW-11, marking shall be applied under the Code Symbol as follows: i.e. RT1, RT2, RT3 etc..
However code case 2235-9 states Name plate shall be marked under code symbol stamp by applying UT (para k of code case)

My understanding is only UT will be stamped on name plate and extent of examination, code case will mentioned on MDR
However we go only by UG116 we can mark RT1 on name plate and specify code case number, extent etc on MDR, I also understand few mfrs specify code case number on name plate too beside RT1

Members please share your opinion and practice followed in your shops.

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mathu.subramanian
Sent: Tuesday, July 22, 2008 10:01 AM
To: materials-welding@googlegroups.com
Subject: [MW:955] RE: 954] CC2235 UT in lieu of RT

Dear Mr. Raghuram,

Beneath RT1, UT to be stamped. (Pl find attached)

Thanks

S.Mathusoothanan
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of RAGHAVENDRA PEMMARAJU
Sent: 22 July, 2008 6:18 AM
To: materials-welding@googlegroups.com
Subject: [MW:954] CC2235 UT in lieu of RT


Dear Raghuram,

Generally we give marking as RT-1 only with a note in Manufacturer's data book (MDR) that UT for so and so seams was carried out in lieu of RT.

regards

rom: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: [MW:951] RE: 949] Re: 939] RE: 931] why CC2235-9 is not applicable for ASMESec.III
To: materials-welding@googlegroups.com
Date: Monday, July 21, 2008, 12:15 PM


Dear Raghavendra
Since you are using CC2235, I have a doubt on Name plate marking as per
UG116 for div 1 vessels. In case when a portion of the vessel RT**ed as
per UW11(a) and the remaining portion UT*ed per CC 2235 in lieu of RT,
what will be the marking, is it RT-1?


From: materials-welding@googlegroups.com [mailto:
materials-welding@googlegroups.com ] On Behalf Of raghavendra
pemmaraju
Sent: Saturday, July 19, 2008 7:34 PM
To: materials-welding@googlegroups.com
Subject: [MW:949] Re: 939] RE: 931] why CC2235-9 is not applicable for
ASMESec.III

Dear Rohit and Raghuram,
Thanks for the information related to Codes,standards and
Specifications.
Our Organisation has obtained 'N' Stamp from ASME during last year and
once the nuclear treaty is signed between India and USA, we have got
bright chances to get orders for manufacture of Nuclear power related
Equipments from abroad.
As we could successfully replace RT by UT as per CC2235 incase of
Sec.VIII vessels, I want the same trend to continue in case of Sec.III
of ASME as well, which are expected in future. But all nuclear new
construction codes of ASME are strong believers in Radiography. I am
looking for a hint to extend TOFD on nuclear new construction also.
That is why my query related to the same.
Hope I could convey.
regards,
Raghavendra

Filtered by Hosted Filtering


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...