Re: [MW:35213] Re: CAN A WELDER QUALIFIED TO ASME IX ALLOWED TO WELD STRUCTURES USING AWS D1.1 PREQUALIFIED WPS

Dear Gents,

As per AWS D.1.1

Para 6.2.2.1 Previous Performance Qualification. 
Previous performance qualification tests of welders , welding operators , and tack welders that are properly documented are acceptable with the approval of the Engineer. The acceptability of performance qualification to other standards is the Engineer 's responsibility, to be exercised based upon
either the specific structure or service conditions , or both.

My opinion consult with client Welding Engineer through (Technical Query or CRM)and resolve

Aravind

On Mon, Sep 2, 2024 at 8:13 AM Naveen Kumar <naveenren@gmail.com> wrote:
Dear Mr. Aneesh,

According to AWS D1.1 2020 - Part 5.1  Welders, welding operators and tack welders that use prequalified WPSs shall be qualified in conformance with Clause 6, Part C or Clause 10, Part D for tubulars.

For Aramco 12-SAMSS-007 section 7.5  Welding procedures and individual welders shall be qualified in accordance with the requirements of AWS D1.1/D1.1M, AWS D1.3, AWS D1.8/D1.8M or AWS D14.1/ D14.1M as appropriate.

If the structural items construction code is AWS D1.1 - Both WPS and Welder Qualification should be as per AWS D1.1 only.

On Saturday, July 13, 2024 at 2:33:54 PM UTC+3 Aneesh K wrote:
Dear Experts

Please advise if a welder qualified in 6G position to ASME Sec IX , is allowed to Weld structures using WPS which is prequalified to AWS D.1.1

Or is it mandatory to perform separate welder qualification using AWS D.1.1 WPS to weld structures 

This is for Saudi Aramco Project

KINDLY ADVICE.

Thanks 


Aneesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f690dfa4-5cb1-4658-aa74-7492c0491d91n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHVAA_fAy4PoyQ11T%2BYdTXeoEyDUp9A9AVYVgP0P5r9GHPs3_Q%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...