Skip to main content

Re: [MW:35211] Reg: Mechanical Testing Failure Analysis

Is there any PWHT

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Sunday 1 September, 2024 at 03:24:46 pm IST, s.navaneethan.mani <s.navaneethan.mani@gmail.com> wrote:


Check the heat input reading for the test coupon.

The mechanical test reading will change If the heat input is high or low from the required values.


Regards
Navaneetha Perumal 

On Fri, 9 Aug 2024 at 9:12 AM, Prathab P <prapoovins@gmail.com> wrote:
Dear Experts,

PQR Test Coupon
Base Plate: A387 Gr22 CL2 (P. No. 5A, Gr.1)
Dimension: 500x350x40mm
Application: Heat Exchanger
Joint Design: Double Bevel

GTAW: Er90SB3
Size: 2.4mm

SMAW: E9018-B3
Size: 3.15 & 4.00mm

Preheating: 160֯C min
Interpass Temp: 200֯C max
DHT: 300֯C for 2hrs

The above mentioned test coupon impact and hardness testing failure. Impact value is getting lower and hardness value getting higher. 

The impact required average value is 55J and hardness max value is 225BHN but the impact actual value getting 22J and the hardness min actual value getting 208BHN.

What is the exert problem for this failure?

Please give us a deeper explanation for this failure. What is the solution?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFyvt4V7Gvpsaa2-01Tj63KBQW-FvqivoAD5JOA0gZj4uCD-VA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOj8udNGOp_CPoexAOdqs%3DKoxNWWqa-AoW%3D%2BtrEZo7BCGW3TXQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...