Skip to main content

Re: [MW:32273] CLAD MATERIALS -WELDING WPS /PQR ERNiCrMo3 / 7018-1 Combination

Dear Sir,

Please Share that WPS.

thank you.

On Wed, Apr 14, 2021 at 8:07 PM pravean ashok <gujulapravean@gmail.com> wrote:
Dear we have in our previous project
Clad material in AlHosan gas Abudhabi and we found there is no issue in that material go a head 


Regards
Pravean

On Wed, 14 Apr, 2021, 11:42 am PK M, <pkmqaqc@gmail.com> wrote:

Hi experts,

 

CLAD MATERIALS -WELDING

 

We have the following Clad Pipe and we are preparing WPS /PQR to weld this SPOOL.

As I know we need to use ERNiCrMo3 / 7018-1 Combination (if GTAW+SMAW) to Complete weld.

But if anyone is having experience with this, please advise whether we will go with

 

GTAW - ER NiCrMo3 ( Root & Hot )

 

SMAW – E7018-1 (Balance Filling /Capping).

 

Please Explain any troubles may have happened regarding dilution or not.

 

Need Aramco and International code reference? If any one has a sample WPS/PQR Please share with us.

 

Any corrosion test or NDT

 

Waiting for your scientific and specific reply.

 

Thanks in Advance.

 

Pkm

pkmqaqc@gmail.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_neYBsYs0Ly8VaMw5SMMw_ueaaAZM4QQs7B_KryHZkjhRQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANO0gODQN_xqMn6tj-oMEv8zh98k9%3DmtUZa-yMDUuFrSxqEncg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nfSkjeBzTeV9DijMOK6G-PttF0uA6b%2B-s8kji%3Dg1%2BmWfw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...