Re: [MW:32203] QW-288 Tube to tube sheet Qualification Essential Variables

ASME Sec. IX Edition 2019
QW-288 Tube to tube sheet Qualification Essential Variables
QW-403 Base Metal

QW-403.31  For tubes of specified wall thickness of 0.100 in. (2.5 mm) or less, a change in tube wall thickness to increase it to more than 2T or to decrease it to less than
1/ 2 T. For tubes of specified wall thickness greater than 0.100 in. (2.5 mm), only one qualification test is required.
Understood.............

Response - Vishwas - I could not locate -   QW-403.31   under  Procedure Qualification   Essential Variable Table - QW 288.1

Please clarify tube OD limits
QW-403.33  A change in the specified tube wall thickness or diameter greater than 10% for all diameters and wall thicknesses.
  Response - Vishwas - The statement is very clear . No issue  of interpretation.Pl. apply/qualify procedure considering  the production welding conditions

Regards




On Sat, Apr 10, 2021 at 8:16 AM pravin.n...@gmail.com <pravin.nimbalkar4@gmail.com> wrote:
ASME Sec. IX Edition 2019
QW-288 Tube to tube sheet Qualification Essential Variables
QW-403 Base Metal

QW-403.31  For tubes of specified wall thickness of 0.100 in. (2.5 mm) or less, a change in tube wall thickness to increase it to more than 2T or to decrease it to less than
1/ 2 T. For tubes of specified wall thickness greater than 0.100 in. (2.5 mm), only one qualification test is required.
Understood.............

Please clarify tube OD limits
QW-403.33  A change in the specified tube wall thickness or diameter greater than 10% for all diameters and wall thicknesses.

Regards,
Pravin Nimbalkar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96449128-c8dd-4230-b6ea-3b7843bad04fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3O-gM-UFMT59OLv3z6Jc%2BSSYiursh3hwt%2B1qxu%3DPmWptQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...