(1) In bracket ( as per QW-452.3 ) mentioned reading belongs to NPS  or OD....??? 
Ans: it clearly mentions OD in mm
(2)Does he is qualified to do welding on 3/4 inch. Pipe With above mentioned range...??
Ans: yes he is qualifying for 3/4 NPS because 3/4 NPS OD is 26.7 mm.



Sent from my iPhone

On 10-Mar-2019, at 9:49 PM, SHERSHA <shershas363@gmail.com> wrote:

Dear Members,

I'm m here to clear  my dout regarding welder qualification diameter range.

With respect to asme sec 9 QW 452.3, a welder test coupon in the range of 1 inch(25) to 2 7/8(73)..he qualified 1 inch(25) and above..[for ref: plz go through ASME SEC-9].

My dout is :-
(1) In bracket ( as per QW-452.3 ) mentioned reading belongs to NPS  or OD....???
(2)Does he is qualified to do welding on 3/4 inch. Pipe With above mentioned range...??

Please help me...

Regads,
Shersha shereef




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...