Friday, March 8, 2019

Re: [MW:29232] What is Deference Between LP & HP welder?

Dear

Please check project specification/vendor procedure/Li censor procedure, nothing given make one letter to client to clarify  

regards

suresh


On Fri, Mar 8, 2019 at 11:10 AM José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
Frankly I had never heard these two concepts, at least they DO NOT EXIST IN ASME, and it did not seem logical to me that they will be linked to a specific type of material. regards!.

El jue., 7 de marzo de 2019 9:47 p. m., Hareesh K V <hareesh13h@gmail.com> escribió:
Dear All, 

At least one person (Mr. José Juan Jiménez Alejandro) asked that question "which is the code?"

To avoid serious before commenting please ask the background.

Which is the construction code? 
ASME B31.1, ASME B31.3 or any other (IBR 1950- India Boiler Regulations )

"May be because of quality issues. Client afraid, interchange the filler wire for HP (P91) LP( P22 or P11)"

In which code it is written that HP is P91 and LP is P22/P11?
HP, LP etc are design basis and cannot be linked to a particular material.

Regards, 

Hareesh K V
+91-8547859202



On Fri, Mar 8, 2019, 6:18 AM José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
CODE???

El jue., 7 de marzo de 2019 10:30 a. m., Arun Kumar.P <arun.ehr@gmail.com> escribió:
Hi,

May be because of quality issues. Client afraid, interchange the filler wire for HP (P91) LP( P22 or P11)

Regards,

Arun

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...