Re: [MW:28008] Re: Using of ER70S-6 in place of ER70S-2

It seems, some kind of trade secret really work behind this phenomena.

On Thu, Jun 28, 2018 at 7:21 PM, Janette Michelle <janettemacias@gmail.com> wrote:
Thanks for your answers. After reviewing the material certs, they all meet the ER70S-6 standard, yet I have my welders saying that one brand of wire burns better over the other brand. What chemical component should I be looking for in terms of how good the wire burns?

On Fri, Jun 8, 2018 at 1:57 AM, Pieper QSI <info@pieper-qsi.nl> wrote:
Most important is what kind of classification / certification is required for the wire and are the by manufacturer specified properties for the wire meeting your project requirements. If during WPQR qualification the requirements also comply with the requirements there is no need to investigate the chemical composition any further as long as the wire is an ER70S-6 wire on the certificate!

Verstuurd vanaf mijn iPhone

Op 7 jun. 2018 om 18:27 heeft Janette M <janettemacias@gmail.com> het volgende geschreven:

Hello,

I need help regarding the ER70S-6 mig welding wire. I am currently comparing mill certs from different vendors and not sure which one is the best in terms of quality. Is there anything in particular I should be looking for?

Any help would be greatly appreciated!


On Tuesday, September 20, 2016 at 6:50:21 AM UTC-5, Diganta Sarma wrote:
Ti and Al are added to act as additional deoxidizers to cleanse the weld of impurities. In the case of MAG welding, additional Ti and Al into the standard ER70S-6 isn't mandated. In case you need them in the weld pool, consider changing the transfer mode to spray or rotating arc or pulsed mode. Some of these will require change of gas to a Argon based mixture

Many thanks!

Sent from my iPhone

On 20 Sep 2016, at 7:43 PM, sanjeev singh <sanjeev...@gmail.com> wrote:

in ER70S6 we have added Ti- 0.011% and Al - 0.012%. We are facing spattering issue in MAG-CO2 .
Is Ti and Al reason for spattering?

Sanjeev 

On Saturday, 17 September 2016 17:39:35 UTC+5:30, sridhar wrote:
You have not mentioned the welding process in use at your end

If it is TIG, flat no. as 70 S2 contains triple deoxidisers Al, ZN & Ti and used with argon gas.
ER 70S06 does not have them and will not give x-ray quality welds.

If it is MAG/CO2 process or with argon gas, you can go ahead. 

Ti addition alone with 70 S6 do not help. S6 also contains excessive Mn & Si and not used for 
TIG process.

Sridhar.


From: sanjeev singh <sanjeev...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Thursday, 15 September 2016 11:40 AM
Subject: [MW:25396] Re: Using of ER70S-6 in place of ER70S-2

Please guide- If we add Ti in ER70S-6 in range of 0.011%, what will be the effect during CO2 welding?

regards,

Sanjeev

On Thursday, 10 January 2013 12:13:36 UTC+5:30, Ranendra Chakraborty wrote:
Dear Expert,
Please guide whether ER70S-6 can be used in place of ER70S-2. Please give code reference.
 
Regards,
Ranendra
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/07c21334-a631-40b0-b66e-65075cde9914%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/52b79f3f-41b6-475b-8d52-c277ae280bfd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...