The Code in previous editions was allowing UT instead of RT for the last joint etc.
Now it is allowed for all cases when the thickness is => 6 mm.
RT1 is symbolizing the extent of RT (or UT). 
Read carefully UG-116(e) and you will not worry about

2018-03-03 20:48 GMT+02:00 venkkatesh krishnan <venkkateshkrishnan@gmail.com>:
Could you share some code related paragraphs of above or any interpretation?. It will helpful to my future reference.

Hope your reply at the earliest.  

On Thursday, March 1, 2018 at 7:49:55 PM UTC+3, George Dilintas wrote:
if it was used in lieu of RT in accordance with Code Requirments, then yes, you can

2018-02-20 15:05 GMT+02:00 venkkatesh krishnan <venkkates...@gmail.com>:
Dear Patrons

Is't permissible to do UT instead of RT on header box whole joint and we possible to mark "RT1" on nameplate as per ASME Sec VIII Div.1?

Looking forward your reply.

Regards,
Venkkatesh Gopalakrishnan.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...