Sunday, March 4, 2018

Re: [MW:27452] P-22 plate welding ...6-MM plate

you have to do control preheating and also cover the same with thermal insulation wool immediately after welding if you are not doing the immediate PWHT,

Regards,

On Sun, Mar 4, 2018 at 2:15 PM, 'Muhammad Asif' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (materials-welding@googlegroups.com) Add cleanup rule | More info

Control maitenance and post heat temperature.

Regards,
Asif


On Fri, Mar 2, 2018 at 10:16 AM, George Dilintas
most probably hydrogen cracking

2018-02-11 12:38 GMT+02:00 pradip kumar Sil <pradipsil@gmail.com>:
Dear Everybody,

We are doing  P-22 plate welding, thickness is 6 mm with E-9018B3 ( Dia 2.5 mm) electrode. Preheat is 150 to 200 degree centigrade with little beveling. Site is near the sea area.

We found lot of delayed crack  generally after 12 hours. Crack is coming middle of the weldment.

Can anybody inform me cause & corrective action for the same. 

Pic attached for your ready reference.

Thanks in advance.
Regards,

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...