Re: [MW:27452] Filler selection

You are going to get hot cracking because of low Ferrite No.
You have to use 309

2018-03-02 12:09 GMT+02:00 Kannayeram Gnanapandithan <kgpandithan@gmail.com>:
No. For dismilar joint between CS to SS, weldmental should have Austenitic structure. When you use 308 directly (19+9) u will not get Austenitic structure due to depletion of Cr plus nickel. So it is better to go for 309(23+12)

On 06-Feb-2018 4:13 pm, "GALAXY INDUSTRIES PRASHANT PANCHAL" <pipanchal@live.com> wrote:
Dear Experts,

Please suggest me that can we use ER308L filler wire for welding Seamless Pipe A312 TP 304 to Coupling A105 or Please suggest the correct one.

With Best Regards, 


Prashant Panchal 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...