Please suggest me the most effective process for brazing of carbide on En 31 material. What are the consumables to be used.
Also suggest me do's and don'ts for the same
On Sat, Mar 3, 2018 at 3:13 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Only difference in impact test temp. But as per ISO impact temp is 6 whereas as per ASME it is 8. Both are marked.--On 02-Mar-2018 10:01 pm, "Perumal Govindan" <perumalgovindan@gmail.com> wrote:Hi
F7A6-EH12K combination is not found on the picture.
The correct filler wire and flux combination for AWS classification F7A6-EH12K is "Union S EH12K - UV C 418TT.
For more information, please refer the attachment.
Regards
P Govindan
On Mar 2, 2018 15:41, "Ankur Pandey" <ankurpandey25@gmail.com> wrote:--Hi,Thanks for replying. Already they have mentioned AWS classification on the manufacturers marking. Please refer attached picture of manufacturer markings on flux bag.I could not find flux wore combination as mentioned in your last mail but what I guess is that you have provided me catalogue with details of flux wire combination as I already have that.Let me know if any other details a required.Regards,Ankur Pandey.On 02-Mar-2018 12:33 PM, "Perumal Govindan" <perumalgovindan@gmail.com> wrote:Hi
Could you please share the filler wire data sheet or batch test certificate, I believe the flux trade name (UV 18 TT) to be changed to get the AWS classification.
Further, please find the attachment for the flux wire combination.
Regards
P Govindan--https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment