Friday, March 2, 2018

Re: [MW:27432] Use of Flux wire combination for SAW welding

Hi, 

Thanks for replying. Already they have mentioned AWS classification on the manufacturers marking. Please refer attached picture of manufacturer markings on flux bag.

I could not find flux wore combination as mentioned in your last mail but what I guess is that you have provided me catalogue with details of flux wire combination as I already have that.

Let me know if any other details a required.

Regards,
Ankur Pandey.

On 02-Mar-2018 12:33 PM, "Perumal Govindan" <perumalgovindan@gmail.com> wrote:

Hi

Could you please share the filler wire data sheet or batch test certificate, I believe the flux trade name (UV 18 TT) to be changed to get the AWS classification.

Further, please find the attachment for the flux wire combination.

Regards
P Govindan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...