Thursday, March 1, 2018

Re: [MW:27413] Re: Narrow groove GMAW - Lack of fusion issues

I would drop it and replace with FCAW

2017-11-12 9:18 GMT+02:00 vinay pawar <vinaypawar02@gmail.com>:

hii
are you facing problem in root or underneath the groove. means root to fill passes.
please specify the job like Dia thk and fit up method like Internal clamp or diffrent.


regards 
Vinay


On Saturday, November 11, 2017 at 5:40:58 PM UTC+3, Harikrishnan Appayi Achari wrote:
Dear All,

We are now facing Lack of Fusion issues with Narrow Groove GMAW (Mechanized Welding). Material is API 5L Grade X60/65. Pipes are having some hi-lo issues too (around 2.5 mm). If anybody came across a similar scenario, kindly share your experience and the way you tackled it.

Thanks and regards,

Hari

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...