Dear experts,
-- MOC - Titanium Grade 2
Tube OD - 20mm
Tube Thickness- 0.9 / 1.1 / 1.2 / 1.8
Query :
Is heat treatment required during bending of titanium tubes to make "U" shape?
If yes, pl share reference for temperature and time to be used and other precautions.
If No, pl share technical reason.