RE: [MW:27096] weld distance for strich welding

Dear Sir,

1. You have not mentioned the construction code.

2. AWS A2.4 is one of the codes, which you can refer the same.

Regards,

Hareesh K V



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Rameez khan RK <rk.rameezkhan21@gmail.com>
Date: 12/3/17 4:07 PM (GMT+05:30)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:27094] weld distance for strich welding

Dear Expert 

                  I would to like to know how to measurement strich welding for more information please see the attachment. So Please any one give me solution for how to check strich welding ( skip welding )

Thanking you
Rameez

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...