Tuesday, November 21, 2017

Re: [MW:27029] Radiography acceptance criteria.

Nice effort sir.
Can this sheet be referred for jobs as per sec VIII Div 1?
Amit 9833859030

On 05-Sep-2013 3:50 PM, "Pradip Ghosh" <pradipg2@gmail.com> wrote:
Dear All,

I have prepared a excel program in which you can find Radiography acceptance criteria of ASME Sec IX,API-650,API-1104,ANSI B 31.3 and ASME Sec VII Div  in a click.
Please give me your review and comments.




Pradip Ghosh

QA/QC Engineer
Mott MacDonald (P) Ltd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...