Re: [MW:22450] Disbonding of clad plate during spinning process

Hi,
Our company spec.(BP) permits acceptance of disbonding upto 1000 mm sq.
Yes the clad is corrosion resistance and service is high pressure hydrocarbon.
On Wednesday, 3 December 2014 13:21:37 UTC+8, sina wrote:
Dear friend
May I ask which code permits dis-bonding in clad? As I guess your clad is corrosion resistance.



On Tue, Dec 2, 2014 at 9:38 AM, MATERIAL <khar...@gmail.com> wrote:
Dear Friends,
 
Noting that every clad mother plate will have some acceptable disbonding,however,spinning/forming of various dish ends can increase it to unacceptable limits.
I would like to ask our gurus about what are the causes of disbonding happening during dish spinning process and how to avoid the same.
 
 
Regards.
 
Ashwani Kumar Khare

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...