Re: [MW:20311] Difference between E-7016 & E-7018

Need not qualify again. If u prepare Weld Map, u can mention the Electrode classification and need not revise WPS

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Wed, Mar 12, 2014 at 9:33 PM, John Henning <jhenning@deltak.com> wrote:

Yes.

Per ASME Section both are qualified; F6, A1 electrodes.  Be sure your WPS states both are allowed.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of anish@contechgroup.net
Sent: Tuesday, March 11, 2014 11:53 PM
To: materials-welding@googlegroups.com
Cc: mails_shankar@yahoo.co.in
Subject: Re: [MW:20302] Difference between E-7016 & E-7018

 

 Hello

 

I am having a PQR qualified with E7018 electrode , and corresponding WPS there by, now i need to qualify some welders for that i need E7016 root and E7018 hot,fill and cap. So i am not changing the essential variables, so is it possible for me to use the same WPS for qualification. can anyone help me in this?

 

Regards

 

Anish

 



On Sunday, December 19, 2010 3:49:29 PM UTC+4, M.Shankar wrote:

Dear Sil,

 

Both are Basic type, low hydrogen rods and having similar strength, but E7016 is without the iron powder in flux.

 

E7016 :Low hydrogen potassium Electrode ( not BASIC SODIUM LOW HYDROGEN; E7015 is Low hydrogen sodium electrode)

E7016's have less slag than E7018's so are better for root-run, positional welding (better controlled positionally) than E7018, easy deslagging and baking/redry not required

 

E7018 :Low hydrogen potassium, iron powder Electrode

E7018 has iron powder added to the flux, which goes into the weld-pool when the rod is burned, so more metal is deposited. Baking/redry required.

 

Both electrodes having F no. 4. You can use E7018 instead of E7016, here essential variable (F no.) not changed, but re-write your WPS accordingly.

 

 

Regards
M.Shankar

 


From: pradip kumar sil <prad...@gmail.com>
To: material...@googlegroups.com
Sent: Sat, 18 December, 2010 7:56:18 PM
Subject: [MW:8784] Difference between E-7016 & E-7018

Dear sir,

What is the quality wise difference between E-7018 ( BASIC LOW HYDROGEN) & E-7016 ( BASIC SODIUM LOW HYDROGEN).Can i use E-7018 insted of E-7016.

Where is the specific area of these two electrode

regards

sil

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...