Dear Binoy:

Preheat is necessary + machining after flame cutting

Do not forget to examine the surface by MT before further application (fit up, welding etc.).
This way, you will detect possible cracks and can grind them out.
 
Regards
Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.kondori@petroyada.com
+98-2123592322
+98-9132150320



On Sun, Mar 9, 2014 at 9:44 AM, Himan Nikdin <himan.nikdin@outlook.com> wrote:
Hi

refer to probability of martensite formation during cutting due to carbon content and alloy element of these kind of steels the hardness may increase to 440 VHN (the base metal hardness is 162~168 VHN) and it will cause to cold crack in base metal, so to prohibit this failure 150 °C preheat + machining after cutting is recommended.

Regards,
Himan Nikdin


Date: Thu, 6 Mar 2014 12:56:39 +0530
Subject: [MW:20242] P22 pipe cutting
From: binoypl3@gmail.com
To: materials-welding@googlegroups.com


Dear All,

Can anyone tell me regarding the cutting of SA 335 P22 pipe cutting procedure.
 
Can we go for Flame cutting or is it mandatory to cut it by Grinding wheel.

Is it mentioned anywhere in standard regarding oxygen flame cutting restriction and the reasons behind this.

If cutting by Oxygen flame is done and if it is not good what corrective action to be taken against this..

--
With Regards
Binoy Lonappan
QAC Engineer
TECCL





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...