There are some discoloration chart available with  Client specification like Shell etc.. which can be used to demonstrate the Level of oxidation on the Root side.
 
Thanks & Regards


J.Gerald Jayakumar
00974-55835810
 
On Saturday, October 19, 2013 9:12 PM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
 
Argon purity level
1. Reactive metals----------99.997%
2. Otherthan reactive metal---99.95%


On Fri, Oct 18, 2013 at 4:28 PM, sevak hiren <hirensevak80@gmail.com> wrote:
Dear Friend,
 
Kindly find my reply as under.
There are three points.
1)    As per ASME section IX, there is no must requirement to mention purity level of shielding Gas. (Judgment based on official ASME interpretation.)
2)    As per ASME Section IIC, SFA 5.32 – Pure argon must be of purity level of 99.99.
3)     Argon up to 99 % purity level may work well, because only 1% or more oxygen can cause weld bead defects. (Judgment based on reading from AWS code D 10.4.)
Conclusion:  For safer practice & considering point no.2, Argon with purity level 99.99 is recommmended.
 
Regards
Hiren Sevak
 
On Wed, Oct 9, 2013 at 9:24 AM, smkabeer ahamed <sm_kabeerahamed@yahoo.co.in> wrote:


On Tuesday, 8 October 2013 11:51 AM, smkabeer ahamed <sm_kabeerahamed@yahoo.co.in> wrote:

Dear friends,

stainless steel welding ss304 to ss304 I have used TIG welding at groove
joint.I have used argon gas purity level 99.7 percent instead of
99.99percent .our client suspect weld joint get oxidized.Is this purity
level is accepted as per any code How we will check what percent of
oxidation available in joint.is any testing method is there.how we will
convince our client and get approval from him.kindly suggest as early as
possible

Regards,

S.M.KABEER AHAMED
CHIEF ENGINEER
QUEST INSPECTION AGENCY
BANGALORE-INDIA


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...