Saturday, October 19, 2013

Re: [MW:18984] Regarding PQR qualification with dissimilar metal

dear sarvanan,
need one clarification here.

if we weld a PQR with Impact Tests with basemetals P No. 1 Gr. 1 ( A 516 Gr. 60 ) to P No.1 Gr. No.2 ( A 516 Gr. 70 ) , then we can write 3 Nos. of WPSs with all supplementary essential variables like P 1 Gr.1 to P 1 Gr.1 , P 1 Gr.1 to P 1 Gr. 2 , P 1 Gr. 2 to P 1 Gr. 2. ? 

can we use these three wps for the job having impact test requirement or for the job without impact test requirement ? 
because for two wps P1 Gr.1 to P1Gr. 1 and P1 Gr.2 to  P1 Gr.2 are having different group numbers then qualified group nos. in PQR.

regards,
sam.




On Thu, Oct 17, 2013 at 6:18 AM, Saravanan Sornam <saravanshyla@gmail.com> wrote:
Hi Vivek ,

You cannot weld separately P1 to P1 Or P8 to P8, because Change of P No. qualified is an essential variable as per QW 403.11, also affecting other Essential Variables, like F No. etc.

You also refer QW 424.1 and its table, just for your knowledge for the base metals used for qualification .

QW-403.5 is purely for Supplementary Essential Variables ( i.e Impact Tests ) for any Group No. changes from the quailfied PQR basemetals , for example , if U weld a PQR with P No.1 Gr .1 to P No. 1 Gr.1, you cannot weld Gr.2. 

But , if you weld a PQR with Impact Tests with basemetals P No. 1 Gr. 1 ( A 516 Gr. 60 ) to P No.1 Gr. No.2 ( A 516 Gr. 70 ) , then you can write 3 Nos. of WPSs with all supplementary essential variables like 
P 1 Gr.1 to P 1 Gr.1 , P 1 Gr.1 to P 1 Gr. 2 , P 1 Gr. 2 to P 1 Gr. 2.

Hope you got the point .

Regards,
Saravanan,
Korea
 


On Wed, Oct 16, 2013 at 9:33 PM, Vivek Pandey <vivek.pande06@gmail.com> wrote:
Dear Sir,

I have doubt something about para QW 403.5 of SEC IX. If i have  qualify a PQR with dissimilar meta llike (P1 TO P8). Can i use the same PQR with same P number like (P1 TOP1 OR P8 TO P8).

Kindly give us your suggestion on same quarry as soon as possible.

Regards.
vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...