Re: [MW:18968] Regarding PQR qualification with dissimilar metal


Dear sir
u can not use this PQR for P1 TO P1 OR P8 TO P8.

with regardes
A.I Shende
GANSONS LTD
NAGPUR -28


On Wed, 16 Oct 2013 18:40:18 +0530 wrote
>Dear Sir,
I have doubt something about para QW 403.5 of SEC IX. If i have  qualify a PQR with dissimilar
meta llike (P1 TO P8). Can i use the same PQR with same P number like (P1 TOP1 OR P8 TO P8).

Kindly give us your suggestion on same quarry as soon as possible.
Regards.vivek



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>
---
>
You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+unsubscribe@googlegroups.com.
>
For more options, visit https://groups.google.com/groups/opt_out.
>
Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35477] WPS for Furnace PWHT

The spools have 1" to 36" Piping joints. The WPS with PWHT is available only for large diameter / high thickness. can we do PWHT i...