Monday, October 7, 2013

Re: [MW:18865] Welder Qualification for Hot-Tapping

On solution is you can weld the entire groove by GTAW (if it is economically acceptable to you and/or thickness is less) and the fillet by SMAW.


On Sun, Oct 6, 2013 at 10:43 PM, LALU RAJENDRAN <lalucpt@gmail.com> wrote:
Dear Mr. Anil

Thanks for your valuable reply. Please heck the below comments

1. Our welders are qualified in 2" SCH 160 pipe, so the qualification range is acceptable for this job.
2. the tapping line is of 2" pipe to be welded on a 24" dia header, and it is very difficult to qualify them in SMAW on a 2" pipe.

Look forward your valuable reply.

Regards, 

LALU R.P


On Sat, Oct 5, 2013 at 2:10 PM, jaya anil <nethalaanil@gmail.com> wrote:
Your welders were already qualified in GTAW + SMAW.

1)  Now just verify the dia in which your welders were qualified,(his qualification range is covering 2"dia )
2)  As welders were qualified in ,Multi process , verifiy the SMAW thickness range of their qualification. whether it is matching with your job requirement.

If above 2 points were matching there is no need of qualifying again, if not you have to qualify them again to meet the Code requirements.




On Fri, Oct 4, 2013 at 1:27 PM, Lalu r p <lalucpt@gmail.com> wrote:
Dear Experts, 

We have a Hot-tapping Job of 2" set-on branch on 42" & 24" Run pipe. Code of construction is B31.3 AND material is SS 321. But our welders are ONLY qualified in GTAW+SMAW. So We need to prepare new WPS and conduct PQR, but my doubt is it mandatory to qualify the welders in SMAW on 2" pipe for this job.Please advise.

Thanks & Regards

LALU R.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
----------------------
Hareesh K V
+91-9447625012


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...