Dear All

We have to do etching on duplex stainless steel pipes as part of the removal of arc strike. Can you please share your experience on the etchants used for this. 

I referred AS 2205.5.1, which describes a) Chrome regia solution, b)  Nitric acid/ hydrochloric acid solution or c) Ferric chloride as etchants for austenitic stainless steels. My doubt is whether it will affect the corrosion resistance of duplex steels.

Thanks and Regards
Harikrishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...