[MW:18890] Partially Claded Reactor Inside dia

For Partially Claded Reactor

Whether we have to consider 

1) Base metal ID of cladded portion as Reactor inside ID or

2) Flushed finished ID

< Query from vendor - For reference >

One vendor considered as below


We have considered base metal ID of cladded portion as
XXXX mm as mentioned in Equipment datasheet.
Request you to confirm that this is base metal ID only & not finished ID.


< Request>

Can any one provide reference drawing for Partially Claded Reactor for better understanding

Expecting reply  09 th Oct 2013


Cheers





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...