I believed you’re refer to pipe use for handrails , normally we always proceed to remove the whole surfaces that appeared like a shiny surfaces or “lacquer” to protect the steel form rusting with grinding or swept blast /2.0 prior sent it the items to galvanizer company. Their always claimed acid doesn’t works to remove it then that were effected in galvanic zinc process.

 

Regards

Mus

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hany alfy
Sent: Monday, 7 October, 2013 6:34 PM
To: materials-welding@googlegroups.com
Subject: [MW:18869] Requirements before Hod Dipped Galvanization

 

 

Dear Experts

 

Is Abrasive blasting is necessary before Hod Dipped Galvanization or can be only Acid Cleaning 

 

Regards,

H.A

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...