Sunday, October 6, 2013

[MW:18856] ASME SECT IX -QW-405.2-Intepretation

Dear Experts

QW-405.2 A change from any position to the vertical position uphill progression. Vertical-uphill progression (e.g., 3G, 5G, or 6G position) qualifies for all positions.

My Take:-
Weld Process - FCAW / Position -2G
Originally 2G PQR qualified without CVN Tests(Supplementary Essential Variable ).But i need to have 2G PQR with CVN Test Results to meet project requirement
I have option of qualify New PQR in 3G with CVN Test. Then i can use 3G CVN Test Result to "upgrade" 2G WPS/PQR.

Pls share your expertise. Thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...