Re: [MW:18792] Re: using of second welder while welding SS material

Ofcourse dharma,
Since you are using 2 welders, 2 various heat inputs, you have to mention in your WPS as the way you have done in PQR. WPS is a work instruction to welding foreman and welders so you must include all technical info in to the WPS , simply not depend on code's essential and supplementary variables.
Saravanan
Korea.

On Sep 28, 2013 1:35 AM, "Dharma dattu" <dharmadattu@gmail.com> wrote:
Dear sir,
my question is that, is this twin tig to be shown in WPS ( is this an essential variable)?

On Sunday, 22 September 2013 16:51:54 UTC+5:30, Dharma dattu wrote:
Dear Experts,
While welding of SS material we need to supply a backing gas, as an alternative a second welder is deployed from back side to support or to melt the weld metal uniformly. is this method to be included in WPS's or is this a general practice. 

Regards,

Dharmadattu.B

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...