Re: [MW:18778] material defect appears during final painting inspection

Dear shashi,

        Its very clearly indicating that you are  not done proper surface preparation during cleaning.  Before painting, suface preparation is very essential integral part of painting . Depending on customer requirement  you have to   blast  clean surface to grade SA2 , SA2-1/2, SA 3, as per ISO8501-01 OR  STS-05 5900 Std or  as per SSPC( Society of structural steel painting council) Std  SSPC-SP-5,SSPC-SP6,SSPC-SP10.etc  Please find attachment for your futher clarification. Which will help you to short out your problem.

Regards.

Manjunath T Madiwalar

Tata Ppower SEd 

Pocess Engineering-Mechanical 

 


On Tue, Sep 24, 2013 at 5:21 PM, shashi <slpo1980@gmail.com> wrote:
Dear Friends,
                      please find the attached showing irregular zig zag profile apperas on the top coat. it seems to be some material defect. please have a look and advice

regards
shashi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...