Dear Anban,

for pipe welding to base plate; this is fillet weld so we can't refer it to note "b".

Note "b" is limited to CJP and PJP like pipe to pipe welding.

Yes, if qualified WPS/PQRs of 1G/2G/3G/4G position(s) can be used to weld any diameter of fillet weld.



-- 
Best regards,
 
Tarek Yehia



On Tue, Sep 24, 2013 at 2:34 AM, Anban <gane2478@hotmail.sg> wrote:

Dear Experts


Table 4.1- WPS/PQR Qulafied x Production Weld Position Qualified Range.

Note "b"- Qualifies for circumferential welds in pipes equal to or greater than 24 in [600 mm] nominal outer diameter

Question - Does "circumferential welds" means only CJP/PJP-girth and seam butt weld joint on inclusive of fillet weld joint,: for example Pipe welding to a base plate?

In my opinion only apply for "only girth and seam butt CJP/PJP weld joint".

My understanding- WPS/PQRs qualified in any of these 1G/2G/3G/4G position(s) can be used to weld any diameter of Circumferential Fillet weld.


Pls advise

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...