Any use of backing  / purging gas in TIG welding process should be mentioned in WPS. including type of gas, its flow rate,
composition level etc.
A second welder can perform  only after grinding the root  to sound weld metal  and not in parallel. This also to be mentioned
in WPS if carried out.

Sridhar.





From: Dharma dattu <dharmadattu@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, 22 September 2013 4:51 PM
Subject: [MW:18734] using of second welder while welding SS material

Dear Experts,
While welding of SS material we need to supply a backing gas, as an alternative a second welder is deployed from back side to support or to melt the weld metal uniformly. is this method to be included in WPS's or is this a general practice. 

Regards,

Dharmadattu.B

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...