Al bronze overlay SMAW Process not possible,

Good to be Either TIG OR GMAW process 

Regards, 

Vidhyapathi 

On 21 Sep, 2013, at 5:03 AM, sarbjeetsingh <sarbsingh.singh@gmail.com> wrote:

Regarding Al- bronze overlay on  alloy steel   by smaw

We are doing al bronze welding on alloy steel  by smaw but lots ot porosity apears   visual in DP check. Can any body sugest proper process or procedure for Al- bronze overlay

Sarbjeet singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...