Sunday, September 22, 2013

Re: [MW:18726] Re: Why pressure drop occur even there was no leakage in hydrostatic test?

Providing more details regarding what is being tested and also the arrangements made would be helpful to give a justifiable reason for the drop in pressure.

In general during hydro testing pressure drop could be basically due to the following 
a) Drop in ambient temperature.
b) Air in the system is not vented out properly during pressurization.

Regards,




On Fri, Sep 20, 2013 at 8:34 AM, mohd <mohd52100@gmail.com> wrote:
dear friends
thanks for posting intersting question

pl specify whether
it is pipeline.U.G or A.G or vessels vertical horizontal
or skid or piping.
what is hydrotest medium n test pressure
pressure guage range

tempeature variation could.not be the only reason for pressure variation.

lets have more info for duscussion.

regards
mohd.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...