Saturday, September 21, 2013

Re: [MW:18725] Welding of SS316L

Main Reasons : Root Gap, Heat Input, Skills of welder, Shielding, Filler wire .

Can i know why are you qualifying WPS with 2mm plate. is it a client requirement, other wise you can go for higer thick ,as WPS will having thickness range.




On Thu, Sep 19, 2013 at 4:57 PM, Krish QA <sarav91k@gmail.com> wrote:

Dear Experts

SS 316L Plate of 2mm welded with ER316L filler wire (1.6mm) using GTAW proceeds with Argon 99.99% for WPS qualification.

After welding we found the following

1.    Centre line crack on root side

2.    Irregular weld profile on root side

Please advice how to medicate these discrepancies.

Regards

Krish

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...