RE: [MW:18723] Re: Welding of SS316L

Hi Krish,

Your weld appears to be heavily oxidized, this normally happens when there is insufficient purge or contaminants.

 

George V Aliyattukudy

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Krish QA
Sent: Friday, September 20, 2013 12:53 PM
To: materials-welding@googlegroups.com
Subject: [MW:18712] Re: Welding of SS316L

 

Please refer attached picture for your review...

 

Regards

 

Krish


On Thursday, September 19, 2013 6:27:03 PM UTC+5:30, Krish QA wrote:

Dear Experts

SS 316L Plate of 2mm welded with ER316L filler wire (1.6mm) using GTAW proceeds with Argon 99.99% for WPS qualification.

After welding we found the following

1.    Centre line crack on root side

2.    Irregular weld profile on root side

Please advice how to medicate these discrepancies.

Regards

Krish

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...