[MW:18802] Option for E6010 in root welding

Dear experts,

1) i want to learn that is there any option of E6010 in root welding of pipe by SMAW available ? i do know that same E6010 used for API 5L grade B, 42 and upto grade 60 also. 

2) If we use E7018 in root (when it suits UTS of base metal) , what is the main problem ? is it only about slag in inside face  and penetration ?

3) Why E6010 is AWS SFA 5.1 and same E7010 is AWS SFA 5.5 (both looks same except UTS) ?

please answer in details.

Regards,
sam.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...