[MW:18791] [MW: 18787]Usage of GTAW and SMAW combination for pipes above 1.5"

Dear experts,
 
Material is Gr.P22 alloy, thickness is less than 13 mm. The WPS which I have for GTAW need PWHT. But since the thickness is less than 13 mm I need to avoid PWHT.
Unfortunately I don't have WPS for GTAW with out PWHT, but I have a GTAW + SMAW wps without PWHT which will cover the required thickness range. Can I use GTAW + SMAW combination for welding 1.5"(7.14 mm thick), 2" (8.74 mm thick) & 3" (11.13 mm thick)pipes.
 
sumod

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...