[MW:18787] Re: using of second welder while welding SS material

Dear Dharmadattu,

Yeah you have to mentioned in WPS.Process Twin tig for Root/hotPasses and same simulation to be done in PQR/WQT.

Regards,

Mohd.



On Sunday, September 22, 2013 2:21:54 PM UTC+3, Dharma dattu wrote:
Dear Experts,
While welding of SS material we need to supply a backing gas, as an alternative a second welder is deployed from back side to support or to melt the weld metal uniformly. is this method to be included in WPS's or is this a general practice. 

Regards,

Dharmadattu.B

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...