Dear experts,
Please clarify our issue ie. In our case clad plate(SA 387 Gr.11
Cl.1+SS 304L), as per our customer spec. Heat treatment of the clad
plate shall be as per applicable clad plate material specification
ie.SA 264 . But our clad plate manufacturer insists that for higher
thickness clad plates heat treatment is not required(ie.46,54,75Thk) &
for lower thickness he will perform heat treatment(ie.24&28Thk). So my
question is as per SA 264 is heat treatment is required or not for
clad plates after explosion bonding and if required which type of heat
treatment is required.
Please clarify my query & thanks in advance for your valuable feedback.
--
With Warm Regards
Krishna Mudhale
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Please clarify our issue ie. In our case clad plate(SA 387 Gr.11
Cl.1+SS 304L), as per our customer spec. Heat treatment of the clad
plate shall be as per applicable clad plate material specification
ie.SA 264 . But our clad plate manufacturer insists that for higher
thickness clad plates heat treatment is not required(ie.46,54,75Thk) &
for lower thickness he will perform heat treatment(ie.24&28Thk). So my
question is as per SA 264 is heat treatment is required or not for
clad plates after explosion bonding and if required which type of heat
treatment is required.
Please clarify my query & thanks in advance for your valuable feedback.
--
With Warm Regards
Krishna Mudhale
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments