[MW:18773] Re: Impact testing failed with ER70S2 wire at -48°C & -35°C

Dear Ali,

If one set is failed you can have/make other set that can be tested.

Which area impact failed HAZ or full weld?

What is base metal spec and thick?

Heat input can be control from 1.8 to 2.1KJ/mm

Filler metal has proven -50ºC tested then filler metal has not issues.

regards,
mohd.






On Sunday, September 22, 2013 12:00:15 PM UTC+3, mhaskar aly wrote:

Dear Friends,

 

I have tested one PQR where Impact testing (GTAW weld) got failed at -48°C & -35°C also;
 
Impact values
9 joules at -48°C
12 Joules at -35°C
 
 
I had received Filler wire with 3.1 certificate having impact tested at-50°C; kindly advise

 

Heat Input max

2.58KJ/mm Root run &

1.8Kj/mm for other runs
 
Kindly advise
 
Ali Mhaskar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...