[MW:18743] FIXTURES TO PREVENT DISTORTION IN WPQT PROCESS

Dear Experts,

We want to qualify New PQRs in various Positions using FCAW-S and SMAW (Different procedures). The details are as follows

Code AWS D1.1

Material – S 355 KT 20

Thickness – 50 mm

The PQR required for immediate cooling after welding. ( 250 Degree to 50 degrees)

I am planning to use Fixtures to prevent distortion.

Is there any restriction to use Fixtures to prevent Distortion in WPQT process ?

Appreciate your advice

Thanks and Regards,

Tomy George

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...