As the dia is small in size there is no need for consumable insert and in tamil nadu welder charges are less than consumable insert. 

For small dia - it is not required and again if u use consumable insert - u may have to apply special technical - equipment - more investment.

small dia full penetration - ( 2 mm root open) generally go for root TIG - here u have to give to which standard u r manufacturing and the WPS varies according to it. 

Who is your customer and what specifically they require all u have to refer.

By stating these things u can ask in the group for some specific WPS also - some ppl are having hundreds of well qualified WPS in their hard disk. 
By stating the above requirements U can request and expect more from the group

On Sat, Nov 17, 2012 at 10:37 AM, Sankaran Sp <subasankaran@yahoo.co.in> wrote:
Dear experts,

We are the leading industrial valve manufacturer in Coimbatore ( INDIA), we have requirement of pipe to pipe "butt joint" welding by TIG process with RT quality.
Pipe materials are ASTM A 335-P91 & A106 Gr B pipe and sizes are 1/2",3/4"& 1"sch 160.
While welding of pipes we need to maintain 2.0 mm root gap with full penetration.
How to carry out this type of welding with RT quality ?
Can you give solution for this requirement?
Can we use consumable inserts between pipes ? If yes  where should get the consumable inserts in INDIA ? who are the suppliers?

Kindly send your recommendations & address.

Advance thanks and regards,
Sankaran.SP
Coimbatore
INDIA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--
Vajjiravelu Ravi
Welding,Painting,NDT & ISO 9001/2008
 
take all steps to save our health  wealth & environment.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...