[MW:15953] SA187 GR11 CL2 Preheat And PWHT of 12 mm PLATE

 Sir,
      I am carrying out a final Year project on Effect of PWHT on "Mechanical properties of Weldmenst of SA387 GR11 Cl2 (Cr1.25%, Mo0.5%)".
      I need to know that is it important to Preheat the Material before welding and how we should arry out welding(Is it Important to carry its root pass from TIG)
      How Many passes we should do for welding the 12 MM plater of this material.
     

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...